| Material: Property vs Dependence | Rank | Popularity (%) | Update date |
|
Yttria stabilized zirconia, YSZ, Zr1-xYxO2-x/2: Resistivity=5.87106e-09 to 1.90274e-06ohm-cm vs Temperature=773 to 1373K
| | 1 | 03/01/2010 |
|
Yttria stabilized zirconia, YSZ, Zr1-xYxO2-x/2: Oxygen diffusion constant=1.20699e-25 to 1.78447e-06cm^2/s vs Temperature=298 to 1273K
| | 1 | 03/01/2010 |
|
BSCCO, Bi2Sr2CaCu2O8+d: Oxygen diffusion constant=6.35272e-19 to 1.65948e-16cm^2/s vs Temperature=263 to 333K
| | 1 | 03/01/2010 |
|
PCMO, Pr0.7Ca0.3MnO3: Oxygen diffusion constant=8.07934e-15 to 3.05879e-13cm^2/s vs Temperature=263 to 333K
| | 1 | 03/01/2010 |
|
Silicon, Si: Infrared refractive index n=3.39015 to 3.43273 vs Temperature=77 to 400K
| | 1 | 02/18/2010 |
|
Titanium dioxide, Titania, TiO2: Resistivity=0.5 to 2.76ohm-cm vs concentration=1.8e+19 to 2e+201/cm^3
| | 1 | 11/04/2009 |
|
Titanium dioxide, Titania, TiO2: Resistivity=25000 to 1e+12ohm-cm vs Temperature=298.15 to 973.15K
| | 1 | 11/04/2009 |
|
Titanium dioxide, Titania, TiO2: Thermal conductivity=11.7 to 11.7Wm/K vs Temperature=273 to 500K
| | 1 | 11/04/2009 |
|
Titanium dioxide, Titania, TiO2: Dielectric constant=85 to 85 vs Temperature=273 to 350K
| | 1 | 11/04/2009 |
|
Titanium dioxide, Titania, TiO2: Dielectric strength=40000V/cm
| | 1 | 11/04/2009 |